Description
Dental waxes and casting defects handwritten notes for bds.
BDS notes for 2nd year
Table of content
Dental waxes
Definition
Classification of waxes according to origin
Classification according to use and application
Composition of dental waxes
Inlay wax
Types of inlay wax
Composition of inlay wax
Desirable properties of wax
Properties of wax
Casting defects
Definition
Classification
Distortion
Surface roughness and irregularities
Porosity
Discoloration
Incomplete casting or missing details