Description
Dental waxes and casting defects handwritten notes for bds.
BDS notes for 2nd year
Table of content
Dental waxes
Definition
Classification of waxes according to origin
Classification according to use and application
Composition of dental waxes
Inlay wax
Types of inlay wax
Composition of inlay wax
Desirable properties of wax
Properties of wax
Casting defects
Definition
Classification
Distortion
Surface roughness and irregularities
Porosity
Discoloration
Incomplete casting or missing details













CBSE Class 9th Social Science Notes PDF
History Notes for BA 3rd Semester in English - Maharshi Dayanand University | Complete Printable Notes
Maharshi Dayanand University | MBA 2nd Semester Entrepreneurship Notes PDF - Complete Printable Notes PDF
BDS 3rd year GENERAL SURGERY handwritten notes PDF
Class 12 Chemistry ( रसायन विज्ञानं ) Printed Notes hindi medium ( with spiral binding )
Class 6 भूगोल (Geography) All Chapters Notes PDF | Hindi Medium | Notes Drive
Maharshi Dayanand University | MCA 2nd Semester Operating System & Shell Programing Notes in English - Complete Printable Notes
Class 8 विज्ञान (Science) All Chapters Notes Pdf | Hindi Medium | Notes Drive
Reviews
There are no reviews yet.